Skip to main content
. 2017 Dec 11;7:17337. doi: 10.1038/s41598-017-17654-x

Figure 9.

Figure 9

XRD patterns of as-quenched specimen and samples non-isothermally tempered to 500 and 650 °C for a medium carbon steel.