The characterization of Ppy deposited on ITO using electrochemical method. (A) morphology of ITO; (B) morphology of Ppy; The insert in A shows the morphology of IDE (both electrode width and spacing between the electrodes of IDEs was 500 μm). (C–F) The charge storage of Ppy IDE characterized by electrochemical measurements. (C) cyclic voltammetric (CV) measurement; (D) current-time curve collected with a pulses signal; (E) the charged charge-voltage curve of Ppy IDE calculated from the time integral of the current in D; (F) the charge-voltage curve at low voltage range. (G and H) showed the adhesion and spreading of MC3T3-E1 cell on ITO electrode and on Ppy electrode after 1 day of culture, respectively.