Skip to main content
. Author manuscript; available in PMC: 2017 Dec 26.
Published in final edited form as: EC Dent Sci. 2017 May 2;2017:52–58.

Figure 2.

Figure 2

Figure 2

Figure 2

SEMs (A) FRC polished smoothly with extremely low wear surface 200X magnification scale bar 100 μm (B) Rough PFC Alert® with debonding microfiber wear surface debris 100X magnification scale bar 200 μm. (C) FRC 5000X magnification reveals how a quartz fiber wears thin into flat plate-like particulate producing the smooth surface in figure 2A, scale bar 5 μm.