Published in final edited form as: ACS Macro Lett. 2017 Aug 31;6(9):1005–1012. doi: 10.1021/acsmacrolett.7b00490

Table 3.

Molecular-weight and concentration information of brush polymer PGMA-g-PEG/PLA and the corresponding micelle Rh and Rg measured by DLS and SAXS, respectively.

Polymer Starting polymer concentration (wt %) Micelle hydrodynamic radius (DLS; nm) Micelle radius of gyration (SAXS; nm) Rg/Rh
PGMA68-g-PEG16/PLA17 0.2 6.9 5.7 0.83
PGMA72-g-PEG45/PLA33 0.27 8.7 6.9 0.79
PGMA72-g-PEG45/PLA33 2 8.7 7.0 0.80
PGMA721-g-PEG45/PLA29 0.27 14.9 17.8 1.19
PGMA721-g-PEG45/PLA29 2 15.8 18.3 1.16