. 2018 Jan 9;8:122. doi: 10.1038/s41598-017-18522-4

Table 1.

Young’s moduli of example microelectrode substrates versus rat brain.

Material Approximate Young’s Moduli (MPa) Refs.
Silicon ~165,000 61
Pt/Ir (90%/10%) ~170,000 62
Cellulose nanocomposite (Pre/Stiff)(Post/Soft) 4,2001.6 40,63
Thiol-ene/acrylateShape Memory Polymer (Pre/Stiff)(Post/Soft) ~2,000~30 28
Rat brain tissue 0.015–0.45 61,64,65

While the methods and values vary in the reported literature, the relative magnitudes are conserved such that Young’s moduli of typical electrode substrates are much greater than polymer-based microelectrode substrates, even dynamically changing materials in their ‘stiff’ state.