. 2017 Nov 30;6(1):668–678. doi: 10.1021/acssuschemeng.7b03026

Figure 6.

Figure 6

(a) DSC traces from the second heating curve with Tg and Tm indicated by the dashed lines and (b) corresponding images showing increase in opacity of BPDA-D polymer with annealing time. Tann = T(tan δMAX) = Tg.