Skip to main content
. 2018 Jan 22;8:1375. doi: 10.1038/s41598-017-18209-w

Figure 4.

Figure 4

Strain cycling test. (a) Experimental setup and (b) customized vise. (c) Relative resistance change every 2000th cycle from the 10,000-cycle test with 4-wt% CNT/PDMS. (d) Change in resistance during 10,000-cycle test with 4-wt% CNT/PDMS. Graphs below represent five cycles around the 100th, 5000th, and 10000th cycle.