XRD pattern of (a) CZTS powders using the conventional hydrothermal process (CHT) at 180 °C for 72 h; (b) MoS2 powder using the CHT process at 200 °C for 24 h; (c) 2:1 ratio of 1 wt% Ag/CZTS and 1T-2H MoS2.