Table 6.

Splitting test results of the test specimen series MDC-M (magnetically driven concrete-steel slag with magnetic orientation).

Specimen 7 Days 28 Days
F (kN) fts (MPa) F (kN) fts (MPa)
MDC-M1 44.1 2.41 47.1 2.57
MDC-M2 43.7 2.39 46.7 2.55
MDC-M3 43.6 2.38 47.3 2.58
MDC-M4 44.3 2.42 46.9 2.56
MDC-M5 44.5 2.43 47.2 2.57
MDC-M6 44.0 2.40 46.8 2.56
Mean 44.0 2.41 47.0 2.57