Skip to main content
. Author manuscript; available in PMC: 2018 Feb 1.
Published in final edited form as: Appl Mater Today. 2016 Jul 29;4:78–82. doi: 10.1016/j.apmt.2016.07.004

Fig. 6.

Fig. 6

SEM image of the electrospun PANI-FLDQV/gelatin fibers. The electrospinning solution contained 2.5% PANI-FLDQV and 10% gelatin. 5 mL of this mixture was electrospun at 14 kV, using 18-gauge needle, delivery rate of 0.8 mL/min, and 12 cm distance from the receiving plate.