Skip to main content
. 2018 Jan 16;18(1):257. doi: 10.3390/s18010257

Table 2.

Results of XRD analysis of the most intensive peaks for commercially available “magnetite” and “strontium hexaferrite” particles.

Particles Type Phases 2θ (˚) FWHMav (˚) Intensity Phases Content (%) DXRD (nm)
“Magnetite” Fe3O4 35.631 0.164 2799.33 94 130
Fe2O3 33.354 0.209 27.61 1 75
FeO(OH) 21.369 0.216 75.64 5 70
“Strontium hexaferrite” SrFe12O19 34.349 0.136 712.19 87 230
Fe2O3 33.319 0.262 166.16 13 50