. 2018 Feb 2;8:2311. doi: 10.1038/s41598-018-19676-5

Figure 1.

Figure 1

Magnetic measured results of 18 nm BFO particles at 50 kOe. Magnetic hysteresis (M-H) loops measured at various temperatures following (a) zero-field cooling (ZFC) and (c) 65 kOe cooling field. Temperature dependent exchange bias field (−HE) under (b) ZFC and (d) 65 kOe cooling field. Insets in (a) and (c) show the local amplification of the corresponding M-H loops.