Table 1. Microtensile Bond Strength (MPa) values (means and standard deviations) of the different experimental groups (*) .

Surface treatment SbU Self-etch SbU Etch-and-rinse
20°C 37°C 20°C 37°C
No (control) 36.14 (6.63)A 32.92 (6.19)A 30.10 (5.93)a 33.78 (4.08)a
Sodium bicarbonate 65.45 (4.46)B 59.53 (11.48)B 49.65 (2.38)b,c 51.44 (7.62)c,d
Aluminum oxide 37.46 (13.42)A 49.67 (7.2)C 44.26 (8.62)b 55.08 (3.74)d
(*)

Similar capital letters (self-etch) and lowercase letters (etch-and-rinse) are not statistically significant (p<0.05)