Skip to main content
. 2017 Dec 15;9(5):6416–6432. doi: 10.18632/oncotarget.23740

Figure 5. Halofuginone-loading in and release from silk films.

Figure 5

Silk films were loaded with Halofuginone via adsorption from solution method as described in the methods section. (A) The resulting Halofuginone loading masses were 6 ± 0.7 μg (low), 13 ± 0.4 μg (middle), 25 ± 1.3 μg (high). (B) Halofuginone release in PBS was monitored via UV spectroscopy (314 nm). All of the Halofuginone release from the low and middle loading groups, and 86% of the Halofuginone release from the high group.