Figure 6.

Figure 6

a) Temporal evolution of diffraction pattern for M1‐doped PSCLC grating in photodynamic process and b) thermodynamic process. c) The rise response time of first‐order diffraction efficiency for M1‐doped PSCLC with different concentration of racemic motor M1 at 80.0 mW cm−2. d) The decay response time of M1‐doped PSCLC at different annealing temperature.