Skip to main content
. 2018 Feb 5;2018:8793481. doi: 10.1155/2018/8793481

Table 3.

Firing steps for heat-treated firing.

Brand Idle temp. (°C) Dry time (s) End temp. (°C) Holding time (min) Heat rate (°C/min) Vacuum Tray open (°C)
Prettau Zirconia 350 5 820 2 55 +
inCoris TZI 350 5 820 2 55 +
Zirlux FC 360 1000 0 55 + 480