Cyclic voltammograms of PEDOT:PSS spin-coated on different numbers of stacked graphene electrodes from G1L to G6L as a function of various scan rates of 5, 10, 20, 30, 40 and 50 mV s−1 in the potential range of −3.0 to 1.5 V. (a) glass/G1L/PEDOT:PSS, (b) glass/G2L/PEDOT:PSS, (c) glass/G3L/PEDOT:PSS, (d) glass/G4L/PEDOT:PSS, (e) glass/G5L/PEDOT:PSS and (f) glass/G6L/PEDOT:PSS.