Characterization parameters of MSNs, MSNs-NH2, MSNs-anti-miR-155, and MSNs-anti-miR-155@PDA-Apt

Sample Sizea (nm) Zeta potential
(mV)
BET surface area (m2/g) Pore volumeb
(cm3/g)
Pore sizec
(nm)
MSNs 125.53±5.46 -16.11±4.25 232.45 0.62 2.83
MSNs-NH2 126.02±3.48 3.11±4.25 227.26 0.59 2.80
MSNs-anti-miR-155 130.57±3.74 -10.57±3.42 157.35 0.38 2.12
MSNs-anti-miR-155@PDA-Apt 182.75±4.76 -15.65±6.26 58.56 0.21

Notes:

a

Nanoparticle size was measured by dynamic light scattering. Data are expressed as mean ± SD.

b

Barrett–Joyner–Halenda (BJH) cumulative pore volume for pores between 1.7 and 300 nm in width.

c

Most probable pore size.

Abbreviations: MSNs, mesoporous silica nanoparticles; PDA, polymerized dopamine; Apt, aptamer; BET, Brunauer–Emmett–Teller; SD, standard deviation; miR-155, MicroRNA-155.