Physical characterizations of GelMA-DOPA hydrogels loaded with different additives. (a) Compressive moduli of GelMA-DOPA hydrogels at different prepolymer concentrations. (b) Compressive moduli of GelMA-DOPA hydrogels of 20% (w/v) prepolymer concentrations with AMP and/or SN additives. (c) Mass swelling of GelMA-DOPA hydrogels at different prepolymer concentrations. (d) Mass swelling of GelMA-DOPA hydrogels of 20% (w/v) prepolymer concentrations with AMP and/or SN additives. (e) In vitro degradation profiles of GelMA-DOPA hydrogels formed at different prepolymer concentrations. (f) Degradation profiles of different hydrogel compositions of 20% prepolymer concentration (*p < 0.05).