Preparation and characterization of NG-DFO. To prepare emulsion templates, the weight ratio of hexane to the aqueous phase was kept at 80:5 and only the AOT to Brij30 ratio as indicated was varied. Note that the weight ratio of AAm to hGMA to PEG-DA was kept at 100:50:25.

NG AOT:Brij30 Diameter,
nm
PDI Zeta, mV
− Fe(III)
Zeta, mV
+ Fe(III)
Mn*
(kDa)
#DFO/NG
NG1-DFO 5:10 36 ± 3 0.08 ± 0.03 − 4.3 ± 0.3 + 1.2 ± 0.3 74 22
NG2-DFO 10:5 101 ± 13 0.17 ± 0.03 − 8.8 ± 0.3 − 8.2 ± 0.2 167 49
*

Apparent number-average molecular weight (Mn) was determined by GPC based on dextran standards