Skip to main content
. 2018 Mar 12;8:4351. doi: 10.1038/s41598-018-22281-1

Figure 8.

Figure 8

Storage modulus before (a) and after (b) annealing at 160 °C and tan delta before (c) and after (d) annealing at 160 °C of scPLA or its composites with varying content of MCH.