Chemical differences analyzed by FTIR: P-O bonds at 570–605 cm−1 and 970–1100 cm−1 as well as O-H bonds at ~3500 cm−1 and 1650 cm−1 were observed in all samples. cerabone® and maxresorb® showed additional hydroxyapatite O-H band around 3575 cm−1. 1460 cm−1, 1420 cm−1, and 880 cm−1 bands were observed for Bio-Oss® and maxgraft® due to presence of CO32− that were not present in cerabone® and maxresorb®. maxgraft® also had absorption bands at 1550 cm−1 and 1245 cm−1 corresponding to C-H and N-H bonds.