. 2018 Feb 8;11(2):259. doi: 10.3390/ma11020259

Figure 2.

Figure 2

Results of SEM examination (original magnification 500×) obtained with BSE and BSE 3D on zirconia surfaces: (A) after grinding (BSE); (B) after grinding (BSE 3D); (C) after blasting with Al2O3110 μm particles under pressure of 0.2 MPa (BSE); (D) after blasting with Al2O3 110 μm particles under pressure of 0.2 MPa (BSE 3D); (E) after blasting with SiC 110 μm particles under pressure of 0.2 MPa (BSE); (F) after blasting with SiC 110 μm particles under pressure of 0.2 MPa (BSE 3D).