Table 1.

A response comparison of as-fabricated sensors in this work with various ZnO nanostructure-based hydrazine sensors.

Electrode Material Sensitivity
(µA·µM−1·cm−2)
Limit of Detection (µM) Linear Range (µM) Response Time (s) Ref.
Nano-nails of ZnO - 0.2 0.1–1.2 <5 [46]
Nanowires of ZnO with high aspect ratio - 0.0847 0.5–1.2 <5 [47]
Nanorods of ZnO 4.76 2.2 0.2–2.0 <10 [48]
Hierarchical micro/nanostructures of ZnO 0.51 0.25 0.8–200 <3 [49]
Nanorods of ZnO/FTO 0.44 515.7 - <10 [50]
ZnO nanorods/alloy 4.48 0.2 - <8 [51]
ZnO nanorods/Single walled carbon nanotube 0.1 0.17 0.5–50 - [52]
Reduced graphene oxide/ZnO-Au 5.54 0.018 0.05–5 <3 [53]
Cetyl pyridine chloride/ZnO 0.172 24 1000–60,000 - [54]
ZnO-1/Au/gold electrode
ZnO-2/Au/gold electrode
ZnO-3/Au/gold electrode
1.70
2.97
1.25
0.25
0.17
0.08
0.8–251
201–851
101–851
<3
<3
<3
[55]