Fig. 1. SEM images of polyluminol–Pt NPs on an ITO chip electrodeposited with different concentrations of H2PtCl6: (A) 9.6 mM; (B) 4.8 mM; (C) 2 mM and (D) 0.5 mM. The electrodepositions were performed in PBS (PH = 2) containing 0.05 M KCl at 60 °C and with an applied potential range from –0.8 V to 0.3 V for 50 cycles at 50 mV s–1 by cyclic voltammetry. (E) ECL curves of the polyluminol–Pt NPs composite film electroplated with different concentrations of H2PtCl6 (0.05–9.6 mM). (F) ECL emission of the polyluminol–Pt NPs composite film electroplated with 0.5 mM of H2PtCl6.