Fig. 5.

Fig. 5

Change in the mechanical properties after accelerated weathering and polyethylene (PE) content correlation; changes in flexural strength (a) and modulus (b) after freeze-thaw cycling test, and tensile strength (c) and modulus (d) after 500 h xenon-arc light weathering.