Figure 3.
Specific loss power (SLP), reported as W/g Fe vs applied magnetic field was measured at fixed frequency (1.50 ± 10 × 105 s−1 kHz) demonstrates surface coating has a minimal impact on the SLP (variations < 10%). The SLP values reported are the mean of all values obtained from a heating measurement that satisfied the (quasi)-adiabatic criteria as described in ref.51 (see text for details). Error bars are the standard deviation of mean values.