Fig. 3. Stability of the three catalyst loadings during galvanostatic experiments at 0.5 A/cm2.

Fig. 3

The stability test was performed under air/H2, 100% RH (cathode/anode). (A) The performance at 0.5 A/cm2 is normalized to the beginning-of-test (BOT) performance at 0.5 A/cm2. (B) Absolute differences in BOT versus end-of-test (EOT) performances.