Skip to main content
. 2018 Jan 3;8(1):2. doi: 10.3390/membranes8010002

Figure 2.

Figure 2

Contact angle and water uptake (%) of the prepared pure chitosan (1 and 2 wt %) and chitosan–gelatin (1:1 g; r = 0.5) blended films/membranes using 1 wt % acetic acid solvent with different concentrations of ferulic acid crosslinker [1.5–6 mM].