Skip to main content
. 2018 Jan 3;8(1):2. doi: 10.3390/membranes8010002

Figure 5.

Figure 5

SEM of the pure 2 wt % chitosan at 1000× (a) and 2000× magnifications (b) and the chitosan–gelatin–ferulic acid (1:1 g; r = 0.5, 3 mM ferulic acid) blended films/membranes using 1 wt % acetic acid solvent at 1000× (c) and 2000× magnifications (d).