Skip to main content
. 2018 Feb 25;11(3):333. doi: 10.3390/ma11030333

Figure 6.

Figure 6

XRD patterns for bovine-derived (a) and synthetic (b) HAp sintered ceramics at 1200 °C for 4 h after 24 h, 72 h and 144 h of exposure to simulated body fluid. Changes in Ca/P ratio (c) and crystallite size (d) obtained by Rietveld refinements.