Skip to main content
. 2018 Feb 27;11(3):349. doi: 10.3390/ma11030349

Figure 2.

Figure 2

Microstructural and morphology details of CEL2 glass-ceramic foams, with 60 wt %, as solid load; (a) cured CEL2 green foam; (b) after firing at 900 °C.