Skip to main content
. 2018 Feb 27;11(3):349. doi: 10.3390/ma11030349

Figure 3.

Figure 3

FTIR analysis of CEL2 glass, green CEL2 glass foams after alkaline activation and CEL2 glass-ceramic foam after firing.