Skip to main content
. 2018 Feb 27;11(3):349. doi: 10.3390/ma11030349

Figure 6.

Figure 6

Examples of CEL2 glass-ceramic foams with different solid content (wt %) and after firing at 900–1000 °C for 1 h; (ac) foams with 58 wt % solid loading fired at 900 °C; (d,e) for foams with 60 wt % solid loading fired at 900 °C; (f) foams with 58 wt % solid loading fired at 1000 °C.