Norton plot of creep rate (s−1) versus stress (MPa) at 1473 K of unalloyed and Si alloyed Laves phases [18,52] and unalloyed A15–Nb3Al [18]. The former are shown in the ∆χ versus VEC maps in Figure 2a,b and the latter in the map in Figure 6 (see text).