Skip to main content
. 2018 Mar 11;11(3):415. doi: 10.3390/ma11030415

Figure 2.

Figure 2

FTIR and EDX spectra, SEM images, and ED patterns of two bioactive glasses before and after being soaked for 7 days in SBF. Left: a P-free glass, GSi–Ca. Right: a glass with analogous composition but including 3 mol-% of P2O5, GSi–Ca–P.