Table 3.

Phase compositions for AA2024 alloy, determined from TEM results from the TEM-226 sample.

Phase Crystal Structure Lattice parameter (Å)
Al12(Fe,Mn)3Si Im3 a = 12.6
Al7Cu2Fe P4/mnc (tetragonal) a = 6.32, c = 14.76
Mg2Si (β) Fm-3m a = 6.34
Al2Cu (θ) I4/mcm (tetragonal) a = 6.03, c = 4.86
AlFeMgSi P6/mmm (hex) a = 6.62, c = 14.63
CuMgAl2 (S) Cmcm a = 3.93, b = 9.42, c = 7.16
Al (α) Fm-3m a = 4.01