Figure 10

Mass loss for rectangular stripes of ferrogels used in MI measurements as a function of time drying in normal conditions (a); Frequency dependence of the maximum value of MI ratio ΔZmax/Z for multilayered structure deposited onto glass substrate. Inset shows field dependence of the ΔZ/Z ratio for characteristic selected frequencies. All units for the layers’ thickness are nanometers (b).