EPD Films HA Portlandite Brushite Calcium Pyrophosphate β-TCP Re:IF-MoS2
Film obtained from solution A 74.8 wt % 25 wt % 0.2 wt %
Film obtained from solution B 17.2 wt % 81.3 wt % 1.5 wt %
Film obtained from solution C 81.1 wt % 17.5 wt % 1.4 wt %
Film obtained from solution A after annealing 73.6 wt % 20.4 wt % 5.9 wt % 0.1 wt %