Composition of the film determined via XRD analysis for different deposition times (from solution A).

EPD films HA Portlandite Calcium Oxide Re:IF-MoS2
Film obtained from solution A without Re:IF-MoS2 (3 h) 87.8 wt % 4.6 wt % 7.6 wt %
Film obtained from solution A (2 h) 82.6 wt % 7.4 wt % 9.1 wt % 0.3 wt %
Film obtained from solution A (3 h) 80.4 wt % 11.3 wt % 8.0 wt % 0.3 wt %
Film obtained from solution A (4 h) 77.8 wt % 13.6 wt % 8.3 wt % 0.3 wt %