. 2018 Apr 3;13:90. doi: 10.1186/s11671-018-2498-1

Fig. 3.

Fig. 3

Cyclic voltammetry profiles of the different catalyst supports, PtRu/TiO2-CNF, PtRu/CNF, PtRu/C, and PtRu/TiO2 in 0.5 M H2SO4 solution at the scan rate of 20 mV s−1