Table 1.
Electrospun templates were fabricated with optimized parameters.
Polymer concentration [mg/mL] | Cl-Am concentration [mg/mL] | Flow rate [mL/h] | Airgap distance [cm] | Applied voltage [+kV] | |
---|---|---|---|---|---|
SD | 65 | 0 | 2 | 13 | 22 |
100 | 1 | 2.5 | 15 | 18 | |
100 | 2.5 | 2.5 | 15 | 18 | |
100 | 5 | 2.5 | 15 | 18 | |
LD | 170 | 0 | 6 | 13 | 22 |
200 | 1 | 3 | 18 | 28 | |
200 | 2.5 | 3 | 18 | 28 | |
200 | 5 | 3 | 18 | 28 |
Polymer and Cl-Am concentration were varied to create two distinct groups of SD and LD templates.