Skip to main content
. 2018 Apr 4;8:5606. doi: 10.1038/s41598-018-23927-w

Figure 13.

Figure 13

SEM image of samples: (a) CuBTA without corrosion, (b) CuBTA after 100 min’s corrosion under 100 μm 3.5 wt.% NaCl TEL, (c) Cu without corrosion and (d) Cu after 100 min’s corrosion under 100 μm 3.5 wt.% NaCl TEL.