Figure 1.

Figure 1

Change in the weight ratio of the PVA-H specimens as a function of the time taken for drying. A weight ratio of 1 means that the weight of the specimen is the same as before drying. (a) shows the results for PVA-H specimens that contain DMSO, and (b) shows the results for those specimens that did not contain DMSO. (mean ± SD, n = 3).