Skip to main content
. 2018 Apr 1;2018:2590536. doi: 10.1155/2018/2590536

Figure 2.

Figure 2

DNA contents and GAG retentions of the DCL. The DNA and GAG contents of DCL under various conditions were measured. The results indicated that the DCL treated with hypotonic 0.5% TE showed the lowest DNA contents (a) and DCL treated with hypertonic 0.5% TE showed the highest GAG contents (b). NC indicates nitrocellulose membrane. Scale bar indicates 50 μm. The values shown are the means ± SEMs (n = 4). Statistical significance: p < 0.05, ∗∗p < 0.005, and ∗∗∗p < 0.005 versus hypotonic 0.5% TE. n.s is not significant.