. 2018 Apr 18;10(2):79–84. doi: 10.4047/jap.2018.10.2.79

Table 1. Fracture strength [in N] after 24 h (37℃) water storage or thermal cycling and mechanical loading (TCML) (mean, standard deviation, minimum, maximum) with adhesive bonding or cementation (identical numbers and letters indicate no significant differences P < .05).

Crown thickness 0.2 mm (group 0.2) Crown thickness 0.5 mm (group 0.5)
Adhesive bonding Cementation Adhesive bonding Cementation
24 hA TCML12 24 h TCML1 24 hB TCML23 24 hAB TCML23
Mean 1164 725 772 0 1628 1430 1357 1510
Std. Deviation 334 809 148 0 174 175 340 792
Minimum 640 0 496 0 1370 1234 899 811
Maximum 1726 1982 932 0 1982 1662 1993 2947