Textural properties of bare AC and as-prepared composite obtained through the LPP process with different iron precursor concentrations

Sample BET Surface Area (m2·g−1) Total Pore Volume (cm3·g−1) Average Pore Size (nm)
Bare AC 1700.7 0.8189 1.9261
NC 1592.6 0.7756 1.8328
IONCC-5 1547.7 0.7691 1.8534
IONCC-10 1504.5 0.7435 1.8670