Figure 4.

Figure 4

The hydrogen evolution rate over the pristine Bi4Ti3O12 and the Bi4Ti3O12−x after chemical reduction treated (a) at 350 °C for various times; (b) at various temperature for 60 min under visible-light irradiation (λ > 400 nm); (c) recycling measure of hydrogen evolution with Bi4Ti3O12−x (350 °C, 60 min) under visible-light irradiation (λ > 400 nm); (d) visible-light photocatalytic hydrogen evolution by fresh Bi4Ti3O12−x (350 °C, 60 min) and Bi4Ti3O12−x (350 °C, 60 min) after four months of storage, compared with the pristine Bi4Ti3O12.