Acceptorless dehydrogenation by Pd@SiCNa

graphic file with name 41467_2018_4143_Figc_HTML.gif

a Reaction conditions: 50 mg (0.18 mol% active metal) Pd@SiCN, 1.0 mmol substrate, 0.75 mL diglyme, 180–200 °C, 18 h (under slight argon flow)

b Yields of isolated products