Skip to main content
. 2016 Dec 20;2(1):10–18. doi: 10.1016/j.bioactmat.2016.12.001

Fig. 5.

Fig. 5

SEM morphologies of pure Fe (a, b), Fe-20CS (c, d), Fe-30CS (e, f) and Fe-40CS (g, h) composites after immersion in SBF for 7 days. Images b, d, f and h present the surface morphology of the corrosion layer at higher magnifications.